Properties Of Spindle Tape
Light, thin, power saving, small elongation after use, long life.
Wear and flexure resistance, oil resistance, and general chemicals resistance.
Moderate friction coefficient, no skid, no debris, small air resistance in operation, spindle speed is stable
Using quick adhesive joint, joint flat, overlapping thickness basically keep the thickness of the belt body.
Specification Of Spindle Tape
Type | Machine type | Spindle speed | Spindle belt reference dimensions(mm) |
Using length | Width | Buy length |
Cotton Spin | FA503 | 8000-18000 | 2840 | 10 | 2870 |
FA506.FA508 | 2625 | 10 | 2655 |
FA507 | 2550-2580 | 10 | 2580、2610 |
FA502.A513C.A513W | 2820 | 10 | 2850 |
FA502A.A513 | 2800 | 10 | 2830 |
Flax
| FX502 | 5000-8000 | 2750 | 17 | 2780 |
FX505 | 2800 | 17 | 2830 |
Chemical fiber | VC443 | 4000-10000 | 0890、2850 | 28、22 | 2920、2880 |
VC8113.VC814 | 3520、3650 | 18、20 | 3550、3680 |
VC432A | 3220 | 22 | 3250 |
ST1202E16S | 2710、2605、2565 | 25 | 2740、2635、2595 |
402 | 3270 | 20 | 3300 |
glass fiber | 210type | 5000-8000 | 2640 | 25 | 2670 |
160type | 2460 | 22 | 2490 |
Application Of Spindle Tape
With easy joint long life, our spindle belt is mainly used in the cotton spinning frame and wool spinning, flax, glass fiber twisting machine and adapted to four spindles, eight spindle, and multiple spindle drive.
How to solve the problem of explosion during rubber mixing?
Cause Analysis:
1. Methanol and ethanol flammable gases are produced;
2. Shear friction produces static sparks;
3. The equipment is not well sealed and the nitrogen protection is not enough.
Measures:
1. Choose a substance that does not produce explosives or has a relatively narrow explosion limit as a dispersant; (effective)
2. The equipment is well sealed; (effective)
3. Fill with nitrogen to isolate oxygen. (effective)
How to solve the problem of inconsistent shrinkage?
Cause Analysis:
1. High low molecular content in the glue;
2. Inconsistent refrigerating time;
3. Inconsistent vacuum time;
4. Inconsistent molecular weight distribution of raw rubber;
5. High volatile content of additives.
Measures:
1. Increase the heating temperature to ensure the vacuum degree and vacuum time;
2. Ensure that the cold and hot refining time of a rubber material is consistent;
3. Make sure that the vacuum time is the same;
4. The same kind of raw rubber is used for the raw rubber;
5. Auxiliaries should be standardized.